Rendered at 08:38:32 GMT+0000 (Coordinated Universal Time) with Cloudflare Workers.
quaffcode 1 hours ago [-]
This is incredible. They blasted 3d waves of alloy through the metal to give different regions different, synergestic properties. And they can adjust those waves to give components different properties at specific locations. The 3d alloying waves itself seems like it could open all kinds of doors. Epic material science win.
lp92 3 hours ago [-]
Doesn't titanium naturally age harden?
metal_am 3 hours ago [-]
No. Aluminum does though
HWR_14 3 hours ago [-]
Does it get more brittle or otherwise have a negative property associated with age? And does Titanium avoid that because it doesn't age harden?
metal_am 2 hours ago [-]
So, lots of things going on here. Natural aging is age hardening at room temperature. Everything in engineering is a tradeoff, so you do lose a little ductility as it gets stronger, but I wouldn't call aluminum in this context brittle.
Some Ti alloys can be age hardened. It's just not going to happen while it's sitting at your desk.
RZhang777 2 hours ago [-]
Turning compositional heterogeneity in LPBF from a defect you try to anneal away into a deliberate design lever is a really clever angle.
From a manufacturing and qualification standpoint, I'm curious how repeatable those microscale Mo waves are across different powder lots and multi-laser builds. Aerospace and medical buyers usually rely on uniform chemistry specs for NDT and lot certification, so qualifying a deliberately heterogeneous microstructure seems like a big hurdle on its own.
Also wondering what a 557 MPa strain-hardening increment does to post-print CNC finish machining—Ti-6Al-4V is already tough on tooling, and rapid work-hardening under the cut could get expensive fast.
Some Ti alloys can be age hardened. It's just not going to happen while it's sitting at your desk.
From a manufacturing and qualification standpoint, I'm curious how repeatable those microscale Mo waves are across different powder lots and multi-laser builds. Aerospace and medical buyers usually rely on uniform chemistry specs for NDT and lot certification, so qualifying a deliberately heterogeneous microstructure seems like a big hurdle on its own.
Also wondering what a 557 MPa strain-hardening increment does to post-print CNC finish machining—Ti-6Al-4V is already tough on tooling, and rapid work-hardening under the cut could get expensive fast.